1. A pool is a corrosion test rig, not just a body of water
Pool water is warm, oxygenated, chlorinated, often salted, and held at a pH that swings between 7.2 and 7.8. The air above it carries chlorine compounds and moisture. Every material in the heat pump is exposed to one or both, continuously, for fifteen years. Corrosion is therefore not an edge case to be handled by a coating; it is a design variable that determines whether the unit still meets its rated capacity in year eight.
2. Four mechanisms and how they show up
Chloride pitting. Free chlorine and chloride ions break down the passive film on stainless and aluminum. It appears as small deep pits, often under deposits, and progresses faster than uniform corrosion because the pit concentrates the chemistry.
Galvanic corrosion. Two dissimilar metals in contact in a wet environment form a cell; the less noble one is consumed. Copper pipe on an aluminum frame, or zinc-plated fasteners on stainless panels, is a designed-in failure.
Under-deposit and crevice attack. Scale, biofilm and gasket crevices trap chlorides and exclude oxygen, which is exactly the condition that defeats the passive film. This is why a scaled exchanger corrodes faster than a clean one, even though the water is the same.
Coating breakdown. A powder coat with a scratch or a poorly prepared edge becomes a site where corrosion undercuts the film, and the panel fails from the inside out.
3. Exchanger materials: why titanium is the default
Titanium resists chlorides at pool temperatures, tolerates the pH band, and does not release copper ions into the water. Copper and copper alloys are attacked quickly; 316L stainless holds up in fresh water but is marginal in high-chloride or salt pools, and fails at crevices and welds.
Two titanium forms are used: tube-in-shell, where water passes through tubes inside a shell of refrigerant, and titanium plate, where thin plates are stacked. Tube-in-shell is more tolerant of particulates, easier to clean mechanically, and thicker-walled; plate packs are compact and efficient but more sensitive to fouling and harder to inspect.
What decides whether a titanium exchanger lasts is not the word titanium but the details: wall thickness, water velocity inside the tubes, pressure drop, and access for cleaning. Low velocity lets sediment settle and biofilm form, which is both an efficiency loss and a corrosion risk. Excessive velocity erodes and raises pump energy. A practical design keeps velocity in a band and fits pressure tappings so that rising differential pressure becomes the cleaning alarm.
4. Fins and casing: the underestimated surfaces
The evaporator coil is aluminum fins on copper tubes in most units, and it sits in the air stream that carries chlorine and moisture. Bare aluminum fins corrode at the fin-to-tube joint, where the contact resistance rises and capacity falls long before a leak appears. Hydrophilic and epoxy coatings slow this down, and in coastal or heavily treated indoor pools they are not optional.
The casing has the same problem at a larger scale. Galvanised sheet with a thin coat is adequate for an inland indoor plant room and fails within a few years on a coast or beside a heavily chlorinated hall. The specification worth asking for is the coating system and its dry film thickness, not just the word “anti-corrosion”.
5. Small parts set the maintenance cost
Fasteners, valve bodies, probe wells, flow switch paddles, drain plugs and cable glands are where corrosion first becomes visible, and where it first becomes expensive. Zinc-plated screws on a stainless panel rust in one season; a brass valve body in a salt pool dezincifies; a steel paddle in a flow switch seizes.
The cheap fix at purchase is to specify stainless fasteners, plastic or stainless wetted parts, and sealed glands. The expensive fix at year four is to dismantle a machine whose bolts no longer turn.
6. Water quality and material combination
| Water condition | Exchanger | Coil and casing | Watch point |
|---|---|---|---|
| Municipal fresh water, pH 7.2–7.8, free chlorine 1–3 ppm | Titanium tube-in-shell | Coated fins, powder-coated frame | Scale control, pH discipline |
| Saltwater pool, 3–5 g/L NaCl | Titanium, thicker wall | Epoxy-coated fins, stainless fasteners | Airborne chlorides on enclosure and frame |
| Hot spring, sulfates and minerals | Titanium, cleanable tube design | Coated coil, sealed enclosure | Deposit formation, cleaning frequency |
| Sea water or brackish make-up | Titanium, highest grade available | Full corrosion package, IP-rated enclosure | Crevice attack at gaskets and welds |
| Poorly maintained pool, low pH | Titanium, but fix the water first | Any coating is at risk | Low pH accelerates every mechanism |
7. Three corrosion myths
- “Titanium means no corrosion problem.” It means the exchanger survives pool water; the coil, frame, fasteners and enclosure are still exposed.
- “A coating solves it.” Coatings delay attack and fail at scratches and edges; the substrate and the drainage path decide the outcome.
- “Water treatment is the pool operator’s issue.” Low pH and high chloride are measured in the pool and paid for in the plant room.
8. The lifetime account
Corrosion spending is small at purchase and large later. The difference between a basic package and a full one is typically a few percent of unit price; the difference in outcome is an exchanger cleaned rather than replaced, a coil that still transfers heat in year six, and fasteners that can be undone during a service visit.
On a coastal or salt-pool project, the calculation is not close. On an inland indoor pool with disciplined water chemistry, a basic package is defensible, provided the coil is cleaned on schedule and the pH is held. The judgment belongs in the specification, before the order, not in a repair quote afterwards.
Related pages in this series
Materials FAQ · Components · Water quality FAQ · Heating process